Hello to all!
I have a question (maybe a simple one) :
Is it possible to bond to platinum using aluminum wire? If it is does
this process needs some special conditions (heating, etc.)
So far I have made some tests and first bond does not stick to the
platinum surface.
Thank you for your help :))